Cloisonné welding wire is made by sprinkling solder powder on the connection between the pinched silver wire and the body, heating it to 800-900℃, melting the solder and then cooling it to firmly bond the silver wire to the body, ensuring the stability of the silver wire and laying the foundation for subsequent processes. |